Primarily for components requiring high strength combined with good ductility and impact strength. Certain design and processing procedures may cause these castings to become susceptible to stress-corrosion cracking.
 

Document History

  1. SAE AMS4236D


    Aluminum Alloy Castings 4.6Cu - 0.35Mn - 0.25Mg - 0.22Ti (A206.0-T4) Solution Heat Treated and Naturally Aged

    • Most Recent
  2. SAE AMS4236C


    Aluminum Alloy Castings, 4.6Cu - 0.35Mn - 0.25Mg - 0.22Ti (A206.0-T4), Solution Heat Treated and Naturally Aged

    • Historical Version
  3. SAE AMS4236B

    👀 currently
    viewing


    Aluminum Alloy, Castings 4.6Cu 0.35Mn 0.25Mg 0.22Ti (A206.0-T4) Solution Heat Treated and Naturally Aged